Dressing and conditioning with mild steel This method is also used tor dressing resin bond CBN wheels (see dressing of resin bonded CBN). |
Surface grinding operating parameters Surface speed vc: 16 to 20 m/s ((3,200 to 4,000 sfpm) Table feed rate vw: 16 to 24 m/min (50 to 75 feetimin) Depth of cut ae: 0.02 mm (0.0008 inch/pass) Cross stroke ap: 60 to 80% of wheel thickness
|
OD cylindrical grinding operating parameters Surface speed vc: 16 to 20 m/s (3,200 to 4,000 sfpm) Speed ratio qs: 60 Depth of cut ae: 0.02 mm (0.0008 inch/pass) Table traverse feed Vfa: 30 to 50% of wheel thickness per revolution
|